Cermet Machining Recommendations
R=Roughing SR=Semi-Roughing SF=Semi-Finishing F=Finishing

Turning & Boring

Material Operation Recommended Grade Speed (SFM) Feed (IPR)
Low Carbon Steels
<Rc35
SR
SR, F
CC-44
CC-42, CC-44
200 - 1,000
200 - 1,200
.006 - .014
.004 - .014
Tool Steels
<Rc35
SR
SF, F
CC-44
CC-42, CC-44
350 - 900
250 - 900
.006 - .014
.004 - .014
Stainless
Steels
SR
SF, F
CC-44
CC-42, CC-44
150 - 750
200 - 900
.004 - .014
.004 - .012
Alloy Steels
<Rc45
SR
SF, F
CC-44
CC-42, CC-44
100 - 1,000
200 - 1,000
.006 - .016
.004 - .013
Cast & Nodular Iron SR
SF, F
CC-44
CC-42, CC-44
200 - 850
200 - 1,200
.008 - .018
.006 - .018
Nickel Based Alloys SF, F CC-42, CC-44 200 - 700 .004 - .010
Powdered Metals SR, R
SF, F
CC-44
CC-42, CC-44
400 - 2,300 .002 - .010
Non-Ferrous Metals SR, R
SF, F
CC-44
CC-42, CC-44
350 - 2,500
450 - 3,300
.006 - .022
.006 - .020
Non-Metallics SR, R
SF, F
CC-44
CC-42, CC-44
300 - 2,100
900 - 2,600
.003 - .014
.002 - .012

Milling

Material Operation Recommended Grade Speed (SFM) Feed (IPT)
Carbon Steels
<Rc35
SR, R
F
CC-43
CC-42, CC-44
300 - 850
450 - 1,150
.002 - .006
.002 - .006
Alloy Steels
<Rc40
SR, R
F
CC-43
CC-42, CC-44
150 - 700
300 - 1,050
.002 - .007
.002 - .005
Tool and
Stainless Steels
SR, R
F
CC-43
CC-42, CC-44
200 - 700
250 - 800
.002 - .006
.002 - .005
Cast Steels SR, R
F
CC-43
CC-42, CC-44
200 - 900
250 - 1,250
.002 - .007
.002 - .005
Cast Iron SF, F CC-44 400 - 1,250 .002 - .005
Nodular Iron SF, F CC-44 150 - 550 .002 - .005

  

Comparison Chart for all Cermet Grades
Chelsea Kennametal Kyocera NTK Sumitomo Teledyne Valenite
CC-42 KT-125 TC-30, 40 T3N, T4N   SD-3 VC-605, 610
CC-43 KT-175 TC-50, 60 XN4 T130A SDM-14 VC-630, 675
CC-44 KT-150 TN-60 XT3 T05A, T12A
T110A, T220A
SD-5 VC-671, 673

  

Properties Chart for all Cermet Grades
Grades Density (G/cm3) Hardness (Ra) T.R.S (Klc)
CC-42 6.5 93.5 6.5
CC-43 6.42 92.0 8.2
CC-44 6.48 92.5 7.5

 

cermetranges.jpg (27354 bytes)